A copper coated wire containing NiCrMo for single pass or multipass welding of low alloy steels.
Designed for welding high yield strength steels with a minimum tensile strength of 770 MPa.
Excellent impact strength at low temperatures down to -40°C.
Ideal for steels requiring tough weld metal for critical applications.
Precision layer wound for superior wire feeding characteristics.
Typically used in the metal working industry, offshore fabrication, chemical & petrochemical industries etc.
Green wire is produced using virgin raw materials sourced from specialised steel mills, which ensures consistent reliability and quality.
Test Certificates can be found online @wilkinsonstar247.com
Typical Base Materials
T1, T1A, T1B, HY90, N-A-XTRA 56-63-65-70, X65, X70, X80, S460, S500, S550, S620, S690, WELDOX 700 etc.*
* Illustrative, not exhaustive list
Standards |
EN ISO 16834-A - G 69 4 M21 Mn3Ni1CrMo |
AWS A5.28 - ER 110S-G |
Chemical Composition % (Typical) | ||||||
C% | Si% | Mn% | P% | S% | Cu% | Cr% |
0.080 | 0.60 | 1.60 | <0.015 | <0.015 | <0.25 | 0.30 |
Ni% | Mo% | Al% | V% | Ti% | Zr% | |
1.50 | 0.30 | <0.030 | 0.10 | <0.050 | <0.050 |
Mechanical Properties (Typical) | ||
Tensile Strength | 800 MPa | |
Yield Strength | 750 MPa | |
Elongation | 19% | |
Impact Strength | 70 J | |
Test Temperature | -40ºC |
Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.
Welding Parameters | ||
Ømm | Current (A) | Voltage (V) |
0.80 mm | 90-160 | 18-22 |
1.00 mm | 150-250 | 22-28 |
1.20 mm | 220-320 | 26-32 |
Shielding Gases
EN ISO 14175 - C1, M20, M21, M33
Welding Positions
EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG
Packaging Data | ||||||||||
Diameter | Weight | Spool | Pallet Qty | |||||||
0.80 mm 1.00 mm Click on any of the following links to download the file. There are no reviews for this product yet. Be the first to add one! |